What you want?
another possibility is that the 100% one took longer to print each layer so layer adhesion was lower(parts in Z direction are about 40-60% weaker already)pla benefits from printing a bit faster/hotter
another possibility is that the 100% one took longer to print each layer so layer adhesion was lower(parts in Z direction are about 40-60% weaker already)pla benefits from printing a bit faster/hotterhttps://www.researchgate.net/publication/351925060_Effect_of_Printing_Parameters_on_the_Thermal_and_Mechanical_Properties_of_3D-Printed_PLA_and_PETG_Using_Fused_Deposition_Modelingalso a bigger diameter nozzle equalized to layer height, though there's controversy if impact strength follows tensile strength https://www.cnckitchen.com/blog/the-influence-of-layer-height-on-the-strength-of-fdm-3d-prints?format=ampthe glass bottle supports are a good idea will make some myself, yesterday i printed these "spray can holders" to save cupboard space
Nice glass!